J506Fe是铁粉低氢钾型药皮的碳钢焊条,交直流两用,可进行全位置焊接。其特点是药皮含有铁粉,可减少焊接层数。
适用于碳钢及低合金钢的焊接,如16Mn等。
J506Fe is Iron powder Low-hydrogen potassium coated carb on steel type electrode. It can be operated in all position welding on both AC and DC.The unique character of the electrode is that Iron powder in eluded in the coati ng, so the welding layer reduced.
It is suitasdble for weldin g of carbon steel a nd low alloy steel, such as 16Mn etc.
| 碳(C) | 锰(Mn) | 硅(Si) | 硫(S) | 磷(P) |
| ≤0.12 | ≤1.6 | ≤0.75 | ≤0.035 | ≤0.040 |
| 试验项目 Test item | 抗拉强度 Tensile strength Mpa | 屈服强度 Yield strength Mpa | 延伸率 Elongation % | 冲击值 Impact value (J)-30°C |
| 保证值 Guaranteed | ≥490 | ≥400 | ≥22 | ≥27 |
| 一般结果 Tested | 520~580 | ≥410 | 24~30 | 50~180 |
| 焊条直径(mm) Weld rod diameter | 2.5 | 3.2 | 4.0 | 5.0 |
| 焊接电流(A) Welding current | 90~120 | 120~150 | 170~200 | 210~250 |
注意事项:
1、焊前焊条须经350°C左右烘焙1小时,随烘随用。
2、焊前必须对焊件清除铁锈、油污、水分等杂质。
3、焊接时须用短弧操作,以窄焊道为宜。
4、用直流电源时,焊条接正极。
Notes:
1.Electrodes must be baked for 1 hour at 350°C before welding operation.
2.It is essential to clean up rusty, oil scale,water and impurities on welding parts.
3.Short arc operation is required when welding. Narrow welding track is proper.
4.Electrode is as positive pole when opration on DC.